Knowledge Resources What is the flexural strength of PTFE? Discover Its Unique Flexibility & Performance
Author avatar

Tech Team · Kintek

Updated 2 weeks ago

What is the flexural strength of PTFE? Discover Its Unique Flexibility & Performance


To be precise, the flexural strength of Polytetrafluoroethylene (PTFE) is approximately 17 MPa (2490 psi). This value indicates the maximum stress the material can withstand in a bending scenario before it yields or breaks. However, this single number only tells part of the story, as PTFE's primary mechanical advantage is its exceptional flexibility and durability, not its rigidity.

The core takeaway is that while PTFE has a high flexural strength, meaning it can bend significantly without breaking, this property is coupled with low stiffness and a tendency to deform under sustained pressure. Therefore, its suitability depends entirely on whether your application requires flexibility and low friction or rigid, load-bearing strength.

What is the flexural strength of PTFE? Discover Its Unique Flexibility & Performance

Deconstructing PTFE's Mechanical Profile

Understanding PTFE requires looking beyond a single data point. Its mechanical behavior is a unique combination of toughness, softness, and unparalleled lubricity.

Flexural Strength vs. Stiffness

Flexural strength measures the ability to resist breaking when bent. PTFE excels here.

In contrast, stiffness (or flexural modulus) measures the ability to resist bending in the first place. PTFE is not a stiff material; its Young's Modulus is quite low, ranging from 0.4 to 0.55 GPa. This is why it feels flexible and pliable rather than rigid.

The Role of Elongation and Impact Strength

PTFE's high flexural strength is a direct result of its ductility. With an elongation at break of up to 400%, it can stretch and deform significantly before failing.

This is complemented by good impact strength (around 160 J/m). It can absorb sudden shocks and impacts without shattering, unlike more brittle plastics.

A Relatively Soft Material

Despite its toughness, PTFE has a low surface hardness of D50-55 on the Shore D scale. This means it is susceptible to scratching and abrasion. While durable in many contexts, it is not considered a hard-wearing material in its unfilled state.

Understanding the Trade-offs: The Challenge of Creep

No material is perfect, and PTFE's primary mechanical limitation is its susceptibility to permanent deformation under load, a phenomenon known as creep or "cold flow."

What is Creep?

Creep is the tendency of a solid material to move slowly or deform permanently under the influence of persistent mechanical stress. For PTFE, this means a component under constant compression, like a seal or gasket, will gradually deform over time.

When Creep Becomes a Problem

This deformation can lead to failure in applications where tight tolerances are critical. For example, a PTFE seal under constant pressure may eventually deform enough to cause a leak. Similarly, a bearing under a continuous load can lose its shape, compromising performance.

Mitigating Creep with Fillers

This weakness can be effectively managed by using filled grades of PTFE. Adding fillers like glass fiber, carbon, or bronze dramatically improves creep resistance, hardness, and wear resistance, making the material suitable for more demanding mechanical applications.

Where PTFE Excels: Unmatched Low-Friction Performance

The defining characteristic of PTFE is its extremely low coefficient of friction, which is often the primary reason for its selection.

An Exceptionally Low Coefficient of Friction

With a coefficient of friction between 0.05 and 0.10, PTFE is one of the most slippery solid materials known. This gives it self-lubricating properties that are essential for high-performance bearings, seals, and non-stick coatings.

The Advantage of Consistent Friction

Crucially, the static (starting) and dynamic (moving) coefficients of friction are nearly identical. This prevents the "stick-slip" phenomenon common in other materials, ensuring a smooth transition from a standstill to motion without jerking.

Making the Right Choice for Your Application

Selecting the right material requires aligning its properties with your primary goal.

  • If your primary focus is dynamic seals or low-friction bearings: PTFE's lubricity is ideal, but consider filled grades to manage wear and creep under sustained loads.
  • If your primary focus is a structural, load-bearing component: Unfilled PTFE is likely unsuitable due to its low stiffness and tendency to creep under pressure.
  • If your primary focus is flexibility and chemical resistance: PTFE's ability to bend without fracturing, combined with its chemical inertness, makes it an excellent choice for flexible tubing, gaskets, or linings.

Ultimately, you should select PTFE not for its absolute strength, but for its unique synthesis of flexibility, chemical resistance, and unparalleled surface lubricity.

Summary Table:

Property Value Key Insight
Flexural Strength ~17 MPa (2490 psi) High resistance to breaking when bent.
Flexural Modulus (Stiffness) 0.4 - 0.55 GPa Low stiffness; material is flexible and pliable.
Coefficient of Friction 0.05 - 0.10 Extremely low, providing self-lubricating properties.
Primary Limitation Susceptible to Creep Can deform under sustained load (managed with fillers).

Need High-Performance PTFE Components?

PTFE's unique combination of flexibility, chemical inertness, and low friction makes it ideal for demanding applications in the semiconductor, medical, laboratory, and industrial sectors.

KINTEK specializes in the precision manufacturing of PTFE components—from custom seals, liners, and labware to complex fabricated parts. We help you leverage PTFE's advantages while mitigating its limitations through:

  • Expert Material Selection: Advising on unfilled or filled grades (e.g., with glass, carbon, bronze) to enhance creep resistance and wear for your specific application.
  • Precision Production & Custom Fabrication: Delivering high-quality parts from prototypes to high-volume orders.

Let's discuss your project requirements and find the optimal PTFE solution. Contact our team today for a consultation!

Visual Guide

What is the flexural strength of PTFE? Discover Its Unique Flexibility & Performance Visual Guide

Related Products

People Also Ask

Related Products

Custom PTFE Parts Manufacturer for Teflon Parts and PTFE Tweezers

Custom PTFE Parts Manufacturer for Teflon Parts and PTFE Tweezers

KINTEK prioritizes precision production and offers custom fabrication from prototypes to high-volume orders.

Custom PTFE Parts Manufacturer for Teflon Containers and Components

Custom PTFE Parts Manufacturer for Teflon Containers and Components

High-precision PTFE containers for labs & industry. Chemical-resistant, customizable sizes. Ideal for semiconductor, medical & lab applications. Get a quote!

Custom PTFE Sealing Tapes for Industrial and High Tech Applications

Custom PTFE Sealing Tapes for Industrial and High Tech Applications

KINTEK's PTFE sealing tape offers superior leak protection, chemical resistance, and high-temperature performance for industrial applications. Custom sizes available.

Custom PTFE Sleeves and Hollow Rods for Advanced Applications

Custom PTFE Sleeves and Hollow Rods for Advanced Applications

High-performance PTFE hollow rods & sleeves for chemical resistance, thermal stability, and low friction. Custom sizes available. Contact KINTEK today!

Custom PTFE Teflon Balls for Advanced Industrial Applications

Custom PTFE Teflon Balls for Advanced Industrial Applications

Precision PTFE balls for chemical, medical & industrial use. High-performance, low-friction, chemical-resistant. Custom sizes available. Get a quote today!

Custom PTFE Square Trays for Industrial and Laboratory Use

Custom PTFE Square Trays for Industrial and Laboratory Use

Premium PTFE square trays for labs & industry. Chemical-resistant, non-stick, high-purity PTFE trays for semiconductors & medical use. Custom sizes available.

Customizable PTFE Rods for Advanced Industrial Applications

Customizable PTFE Rods for Advanced Industrial Applications

High-performance PTFE solid rods for chemical-resistant, low-friction components. Ideal for lab, medical & industrial applications. Custom machining available.

Custom PTFE Bottles for Diverse Industrial Applications

Custom PTFE Bottles for Diverse Industrial Applications

High-purity PTFE bottles for chemical storage, resistant to acids & solvents. Wide/narrow mouth options, leak-proof, durable. Ideal for labs & industry.

Customizable PTFE Seals Filter Holders for Versatile Applications

Customizable PTFE Seals Filter Holders for Versatile Applications

Enhance filtration with KINTEK's PTFE-sealed filter holders for leak-proof, chemical-resistant performance in labs and industries. Explore now!

Custom PTFE Volumetric Flasks for Advanced Scientific and Industrial Use

Custom PTFE Volumetric Flasks for Advanced Scientific and Industrial Use

Premium PTFE volumetric flasks for labs – chemical-resistant, non-stick, precise measurements. Ideal for semiconductor, medical & analytical applications. Shop now!

Custom PTFE Measuring Cylinders for Advanced Scientific and Industrial Applications

Custom PTFE Measuring Cylinders for Advanced Scientific and Industrial Applications

Discover the superior performance of our Polytetrafluoroethylene (PTFE) measuring cylinders, engineered for precision and resilience in demanding environments.

Customizable PTFE Crucibles for Laboratory and Industrial Applications

Customizable PTFE Crucibles for Laboratory and Industrial Applications

High-purity PTFE crucibles with lids for labs. Chemical-resistant, non-stick, and durable. Ideal for sample digestion, AA, ICP-MS. Custom sizes available.

Custom PTFE Evaporating Dishes for Diverse Applications

Custom PTFE Evaporating Dishes for Diverse Applications

High-purity PTFE evaporating dishes for labs, resistant to acids & solvents. Non-stick, durable, ideal for sample prep. Custom sizes available. Order now!

Custom PTFE Teflon Parts Manufacturer PTFE Magnetic Stirring Bar

Custom PTFE Teflon Parts Manufacturer PTFE Magnetic Stirring Bar

KINTEK PTFE magnetic stirring bars offer chemical resistance, high-temperature stability, and smooth mixing for labs. Ideal for diverse applications.

Custom PTFE Microwave Digestion Vessels for Demanding Applications

Custom PTFE Microwave Digestion Vessels for Demanding Applications

High-purity PTFE microwave digestion vessels for safe, contamination-free sample prep. Ideal for ICP-MS, AAS, and trace analysis. Custom sizes available.

Custom PTFE Teflon Parts Manufacturer Conductive Glass Substrate Cleaning Rack

Custom PTFE Teflon Parts Manufacturer Conductive Glass Substrate Cleaning Rack

High-purity PTFE flower baskets for lab cleaning, resistant to chemicals & extreme temps. Custom designs available for semiconductor & medical applications.

Custom Machined Molded PTFE Teflon Parts Manufacturer for Laboratory ITO FTO Conductive Glass Cleaning Flower Basket

Custom Machined Molded PTFE Teflon Parts Manufacturer for Laboratory ITO FTO Conductive Glass Cleaning Flower Basket

High-purity PTFE flower baskets for semiconductor & lab use. Chemical-resistant, custom designs available. Ideal for silicon wafers & glass substrates.

Custom PTFE Teflon Parts Manufacturer PTFE Cleaning Rack

Custom PTFE Teflon Parts Manufacturer PTFE Cleaning Rack

High-purity PTFE flower baskets for labs & semiconductor use. Chemical-resistant, -180°C to +250°C, custom sizes available. Contact KINTEK today!

Custom PTFE Teflon Parts Manufacturer Adjustable Height Flower Basket

Custom PTFE Teflon Parts Manufacturer Adjustable Height Flower Basket

High-purity PTFE adjustable height flower baskets for semiconductor and lab use. Chemical-resistant, non-stick, and customizable. Get yours today!

Custom PTFE and Nitrile Diaphragm Pump Components for Demanding Applications

Custom PTFE and Nitrile Diaphragm Pump Components for Demanding Applications

High-performance PTFE & Nitrile replacement balls and seats for QBY/QBK pumps. Chemical-resistant, durable, and precision-engineered for optimal pump efficiency.


Leave Your Message